Sealing the Hull


Rolling on Bote Cote Marine Epoxy Resin.  
We recommend cheap foam roller skins when applying to large areas. 
Do NOT play with it too much to minimise air bubbles.
Finish after three (3) coats of Bote Cote applied.
First coat applied with 20% Timber Preservative and Reactive Diluent Agent (TPRDA) added.


Note all screw heads and cracking have been filled and faired before applying Bote Cote.